Copper alloys — Ammonia test for stress corrosion resistance
Primary tabs
Reference:
ISO 6957:1988
Publication Year:
1988
Domain:
Specifies a test, using an ammoniacal atmosphere, for the detection of applied or residual stresses which can cause failure of the material in service or storage through stress corrosion cracking. The severity of the method can be regulated by changing the pH value. In an informative annex, recommendations are given for the choice of pH-values.
28 000 F CFA